Back

Features and Benefits

  1. Improved bond strength for secure installations
  2. No curing required after block work is completed
  3. Flexible, shock and impact resistant
  4. Provides optimum compressive and splitting tensile strength
  5. Easy to use with long working time
  6. Fast and economical application
  7. Superior adhesion and consistent quality
  8. Advanced technology with longer pot life
  9. Reduces material wastage

Suitable Substrates

  1. AAC Blocks
  2. Cement Mortar Blocks/Bricks
  3. Concrete Hollow Blocks
  4. Lightweight Masonry Blocks
  5. Cellular Concrete Blocks
  6. Fly Ash Bricks
  7. Calcium Silicate Bricks
  8. Clay Bricks
ASTM C 1660 Data
#PropertyTest MethodRequirementTypical Values
1Splitting Tensile StrengthASTM C166058-71 psi (0.40-0.49 MPa)50-70 psi
ASTM C 270 Data
#PropertyTest MethodRequirementTypical Values
1Compressive StrengthASTM C109Minimum 750 psi (5.2 MPa)850-950 psi
2Water RetentionASTM C1506Minimum 75%85%-90%
3Air ContentASTM C91Maximum 14%10%-12%
Mortar Bed Thickness Coverage for 50 Kg Bag Coverage for 20 Kg Bag
12mm300sft120sft
23mm200sft80sft
34mm150sft60sft

Technical Data Sheet

Material Safety Data Sheet